QH-2/h Metal Powder Spray Welding Torch |
![]() |
![]() |
Metal powder spray welding gun: Use
method 1st-step: with oxygen acetylene flame on the work piece is heated to 300--400 degrees Celsius. 2nd-step:The nozzle and the workpiece surface distance 120~150 mm, at same time you can put the self fluxing alloy powder evenly sprayed on the surface of the workpiece, and then through the flame to melt, to appear on the surface mirror, gradually moving molten position, so that the alloy powder and the workpieces mutually cladding, dispersed to each other to form a binding layer firmly. 3rd-step: different kinds of alloy powder used, can get the abrasion resistance, corrosion resistance and other different properties of strengthened layer. |
![]() |
![]() |
Spray gun, if no ignition, can not press powder valve switch, to avoid blockage . |
Due to the powder 's particle size is not uniform, or become damp and other factors, make the powder valve switch failure, clogging, it should be repaired in time before be used again . |
Regular cleaning spray gun, in order to avoid the gas tube holes are blocked. while cleaning pipe hole ,ejects out and clean up the control powder feeder. |
Spray gun at the end of work, first close the acetylene valve, and then use the oxygen blowing internal pipeline, after liquidation shall be sprayed welding torch and hose hanging, prevent dust and impurity invasion of spray welding nozzle, to effect the normal use. |
All the pipelines of spray welding torch are not contaminated oil, to prevent oxygen meet oil to have combustion and explosion . |
![]() |
![]() |
![]() |
![]() |